Steel · Stainless steel, austenitic · isotropic

1.4318 (X2CrNiN18-7)

EN 1993-1-4 · EN 10088 · annealed (nominal design values) · also X2CrNiN18-7

1.4318 (X2CrNiN18-7) is an austenitic stainless steel to EN 1993-1-4 · EN 10088. Its nominal yield strength is 330–350 MPa, depending on the product form and thickness. E = 200 GPa, ν = 0.3 and α = 16 × 10⁻⁶/K (design values).

Record
stainless-14318
Library
v1.1.0
Properties
10
Sources
2
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 200GPa design[1]
ν · Poisson's ratio 0.3– design[1]
f_y · Yield strength (R_eH / R_p0.2) 350MPa nominal[1]C · t ≤ 8 mm
f_u · Tensile strength (R_m) 650MPa nominal[1]C · t ≤ 8 mm
ρ · Density 7900kg/m³ typical[2]
α · Coefficient of thermal expansion 1610⁻⁶/K typical[2]
λ · Thermal conductivity 15W/(m·K) typical[2]
c_p · Specific heat capacity 500J/(kg·K) typical[2]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus ⓘ EN 1993-1-4 2.1.3 200 GPa design [1]
ν Poisson's ratio 0.3 – design [1]
G Shear modulus ⓘ G = E/(2(1 + ν)); SCI P413 rounds it to 76.9 GPa for 200 GPa 76.92 GPa derived [1]
K Bulk modulus K = E / 3(1 − 2ν) 166.7 GPa derived —
λ_L Lamé constant λ_L = Eν / (1 + ν)(1 − 2ν) 115.4 GPa derived —
c₀ Bar wave speed c₀ = √(E/ρ) 5032 m/s derived —

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density ⓘ EN 10088-1 values as quoted by Outokumpu 7900 kg/m³ typical [2]
α Coefficient of thermal expansion ⓘ mean, 20–100 °C 16 10⁻⁶/K typical [2]
λ Thermal conductivity ⓘ at 20 °C 15 W/(m·K) typical [2]
c_p Specific heat capacity ⓘ at 20 °C 500 J/(kg·K) typical [2]
ρ_e Electrical resistivity ⓘ at 20 °C 0.73 µΩ·m typical [2]
a Thermal diffusivity a = λ / (ρ·c_p) 3.797 mm²/s derived —

Strength

a band applies up to and including its upper limit
PropertyProduct formThicknessValueUnitBasisRef.
f_yC — cold rolled stript ≤ 8 mm350MPanominal[1]
f_yH — hot rolled stript ≤ 13.50 mm330MPanominal[1]
f_yP — hot rolled platet ≤ 75 mm330MPanominal[1]
f_uC — cold rolled stript ≤ 8 mm650MPanominal[1]
f_uH — hot rolled stript ≤ 13.50 mm650MPanominal[1]
f_uP — hot rolled platet ≤ 75 mm630MPanominal[1]
SymbolPropertyValue at t = 8 mm · CUnitBasisRef.
f_y Yield strength (R_eH / R_p0.2) ⓘ 0.2 % proof strength, EN 1993-1-4 Table 2.1 350 MPa nominal [1]
f_u Tensile strength (R_m) 650 MPa nominal [1]

Sources

every value names one
  1. EN 1993-1-4:2006+A1:2015, Eurocode 3 — Stainless steels, Table 2.1 and 2.1.3Copies checked: 1, 2
  2. EN 10088-1, Stainless steels — List of stainless steels, physical properties (as quoted by Outokumpu datasheets)Copies checked: 1, 2, 3, 4

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). 1.4318 (X2CrNiN18-7) — material properties, EN 1993-1-4 · EN 10088. Library v1.1.0, record stainless-14318. https://badgermecx.com/materials/stainless-14318/ (accessed 2026-10-08).

@misc{badgermecx_stainless14318,
  title  = {1.4318 (X2CrNiN18-7) -- material properties, EN 1993-1-4 · EN 10088},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record stainless-14318},
  url    = {https://badgermecx.com/materials/stainless-14318/}
}

Export and related

SI units, every value with basis and source