Titanium · Titanium alloy · isotropic

Ti-6Al-4V (grade 5)

ASTM B265 grade 5 · annealed

Ti-6Al-4V (grade 5) is a titanium alloy to ASTM B265 grade 5. Its minimum yield strength is 828 MPa. E = 107 GPa, ν = 0.31 and α = 9 × 10⁻⁶/K (typical values).

Record
ti-6al-4v
Library
v1.1.0
Properties
10
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 107GPa typical[1]
ν · Poisson's ratio 0.31– typical[1]
f_y · Yield strength (R_eH / R_p0.2) 828MPa min[1]
f_u · Tensile strength (R_m) 895MPa min[1]
ρ · Density 4420kg/m³ typical[1]
α · Coefficient of thermal expansion 910⁻⁶/K typical[1]
λ · Thermal conductivity 6.6W/(m·K) typical[1]
c_p · Specific heat capacity 580J/(kg·K) typical[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus 107 (107 – 122) GPa typical [1]
G Shear modulus 41 (41 – 45) GPa typical [1]
ν Poisson's ratio 0.31 – typical [1]
K Bulk modulus K = E / 3(1 − 2ν) 93.86 GPa derived —
λ_L Lamé constant λ_L = Eν / (1 + ν)(1 − 2ν) 66.63 GPa derived —
c₀ Bar wave speed c₀ = √(E/ρ) 4920 m/s derived —

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density 4420 kg/m³ typical [1]
α Coefficient of thermal expansion ⓘ 0–100 °C 9 10⁻⁶/K typical [1]
λ Thermal conductivity 6.6 W/(m·K) typical [1]
c_p Specific heat capacity 580 J/(kg·K) typical [1]
ρ_e Electrical resistivity ⓘ at 0 °C 1.68 µΩ·m typical [1]
a Thermal diffusivity a = λ / (ρ·c_p) 2.575 mm²/s derived —

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_y Yield strength (R_eH / R_p0.2) ⓘ annealed sheet and plate, ASTM B265 828 MPa min [1]
f_u Tensile strength (R_m) ⓘ annealed sheet and plate, ASTM B265 895 MPa min [1]

Sources

every value names one
  1. TIMET datasheets: TIMETAL 50A (CP grade 2) and TIMETAL 6-4 (Ti-6Al-4V)Copies checked: 1, 2

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). Ti-6Al-4V (grade 5) — material properties, ASTM B265 grade 5. Library v1.1.0, record ti-6al-4v. https://badgermecx.com/materials/ti-6al-4v/ (accessed 2026-11-26).

@misc{badgermecx_ti6al4v,
  title  = {Ti-6Al-4V (grade 5) -- material properties, ASTM B265 grade 5},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record ti-6al-4v},
  url    = {https://badgermecx.com/materials/ti-6al-4v/}
}