Titanium · Titanium · isotropic

Titanium grade 2 (CP)

ASTM B265 grade 2 · annealed

Titanium grade 2 (CP) is a commercially pure titanium to ASTM B265 grade 2. Its minimum yield strength is 275 MPa. E = 105 GPa and α = 8.6 × 10⁻⁶/K (typical values).

Record
ti-grade2
Library
v1.1.0
Properties
7
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 105GPa typical[1]
f_y · Yield strength (R_eH / R_p0.2) 275MPa min[1]
f_u · Tensile strength (R_m) 485MPa typical[1]
ρ · Density 4510kg/m³ typical[1]
α · Coefficient of thermal expansion 8.610⁻⁶/K typical[1]
λ · Thermal conductivity 21.79W/(m·K) typical[1]
ρ_e · Electrical resistivity 0.53µΩ·m typical[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus 105 (105 – 120) GPa typical [1]

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density 4510 kg/m³ typical [1]
α Coefficient of thermal expansion ⓘ 20–100 °C 8.6 10⁻⁶/K typical [1]
λ Thermal conductivity 21.79 W/(m·K) typical [1]
ρ_e Electrical resistivity ⓘ temperature not stated 0.53 µΩ·m typical [1]

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_y Yield strength (R_eH / R_p0.2) 275 MPa min [1]
f_u Tensile strength (R_m) ⓘ typical; the minimum is not quoted here 485 MPa typical [1]

Sources

every value names one
  1. TIMET datasheets: TIMETAL 50A (CP grade 2) and TIMETAL 6-4 (Ti-6Al-4V)Copies checked: 1, 2

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). Titanium grade 2 (CP) — material properties, ASTM B265 grade 2. Library v1.1.0, record ti-grade2. https://badgermecx.com/materials/ti-grade2/ (accessed 2026-11-26).

@misc{badgermecx_tigrade2,
  title  = {Titanium grade 2 (CP) -- material properties, ASTM B265 grade 2},
  author = {{BadgerMecX Materials}},