Aluminium · Aluminium, conductor and sheet grade · isotropic

EN AW-1050A O/H111

EN 485-2 · soft (O/H111) sheet

EN AW-1050A O/H111 is an aluminium grade for conductors and sheet to EN 485-2. Its minimum 0.2 % proof strength is 20 MPa. E = 69 GPa and α = 23.5 × 10⁻⁶/K (typical values).

Record
al-1050a-o
Library
v1.1.0
Properties
7
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 69GPa typical[1]
f_o · 0.2 % proof strength 20MPa min[1]
f_u · Tensile strength (R_m) 65MPa min[1]
ρ · Density 2700kg/m³ typical[1]
α · Coefficient of thermal expansion 23.510⁻⁶/K typical[1]
λ · Thermal conductivity 210W/(m·K) typical[1]
σ_e · Electrical conductivity 34MS/m typical[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus 69 GPa typical [1]

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
α Coefficient of thermal expansion ⓘ 20–100 °C 23.5 10⁻⁶/K typical [1]
ρ Density 2700 kg/m³ typical [1]
λ Thermal conductivity ⓘ lower end of the datasheet range 210 (210 – 220) W/(m·K) typical [1]
σ_e Electrical conductivity ⓘ lower end of the datasheet range 34 (34 – 36) MS/m typical [1]

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_o 0.2 % proof strength ⓘ R_p0.2 ≥ 20 MPa, EN 485-2 20 MPa min [1]
f_u Tensile strength (R_m) ⓘ R_m 65–95 MPa, EN 485-2 65 (65 – 95) MPa min [1]

Sources

every value names one
  1. Wieland aluminium datasheets: EN AW-1050A, 5083, 6061, 6082Copies checked: 1, 2, 3, 4

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). EN AW-1050A O/H111 — material properties, EN 485-2. Library v1.1.0, record al-1050a-o. https://badgermecx.com/materials/al-1050a-o/ (accessed 2026-11-26).

@misc{badgermecx_al1050ao,
  title  = {EN AW-1050A O/H111 -- material properties, EN 485-2},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record al-1050a-o},
  url    = {https://badgermecx.com/materials/al-1050a-o/}
}

Export and related

SI units, every value with basis and source