1.4301 (X5CrNi18-10) vs 1.4318 (X2CrNiN18-7)

1.4318 (X2CrNiN18-7) and 1.4301 (X5CrNi18-10) are about equally stiff. Their densities are about the same. Per unit mass they are about equally stiff (25.32 and 25.32 MJ/kg). Strength: f_y = 230 MPa for 1.4301 (X5CrNi18-10), f_y = 350 MPa for 1.4318 (X2CrNiN18-7).

Side by side

ratio = 1.4318 (X2CrNiN18-7) / 1.4301 (X5CrNi18-10) · log scale
Property 1.4301 (X5CrNi18-10) 1.4318 (X2CrNiN18-7)UnitRatio¼×1×4×
E Young's modulus 200 200 GPa 1×
G Shear modulus 76.92 76.92 GPa 1×
ν Poisson's ratio 0.3 0.3 – 1×
ρ Density 7900 7900 kg/m³ 1×
α Coefficient of thermal expansion 16 16 10⁻⁶/K 1×
λ Thermal conductivity 15 15 W/(m·K) 1×
c_p Specific heat capacity 500 500 J/(kg·K) 1×
ρ_e Electrical resistivity 0.73 0.73 µΩ·m 1×
f_y Yield strength (R_eH / R_p0.2) 230 350 MPa 1.52×
f_u Tensile strength (R_m) 540 650 MPa 1.2×
E/ρ Specific stiffness E/ρ · derived 25.32 25.32 MJ/kg 1×
c₀ Bar wave speed √(E/ρ) · derived 5032 5032 m/s 1×
f/ρ Specific strength f/ρ · derived 29.11 44.3 kJ/kg 1.52×

Values at the first thickness band or product form of each material (EN 1993-1-4 · EN 10088 · t ≤ 8 mm · C; EN 1993-1-4 · EN 10088 · t ≤ 8 mm · C). A minimum and a characteristic value are not the same kind of number — read the ratio as a guide. Each material's page lists every band and every source.