C80/95 is 1.2 times as stiff as C45/55. Their densities are about the same. Per unit mass C80/95 is 1.2 times as stiff. Strength: f_ck = 45 MPa for C45/55, f_ck = 80 MPa for C80/95.
Side by side
ratio = C80/95 / C45/55 · log scale| Property | C45/55 | C80/95 | Unit | Ratio | ¼×1×4× |
|---|---|---|---|---|---|
| E Young's modulus | 36 | 42 | GPa | 1.17× | |
| G Shear modulus | 15 | 17.5 | GPa | 1.17× | |
| ν Poisson's ratio | 0.2 | 0.2 | – | 1× | |
| ρ Density | 2447 | 2447 | kg/m³ | 1× | |
| γ Weight density | 24 | 24 | kN/m³ | 1× | |
| α Coefficient of thermal expansion | 10 | 10 | 10⁻⁶/K | 1× | |
| f_ck Characteristic cylinder strength | 45 | 80 | MPa | 1.78× | |
| f_ck,cube Characteristic cube strength | 55 | 95 | MPa | 1.73× | |
| f_cm Mean cylinder strength | 53 | 88 | MPa | 1.66× | |
| f_ctm Mean tensile strength | 3.8 | 4.8 | MPa | 1.26× | |
| f_ctk,0.05 Tensile strength, 5 % fractile | 2.7 | 3.4 | MPa | 1.26× | |
| f_ctk,0.95 Tensile strength, 95 % fractile | 4.9 | 6.3 | MPa | 1.29× | |
| ε_c1 Strain at peak stress | 2.4 | 2.8 | ‰ | 1.17× | |
| ε_cu1 Ultimate strain | 3.5 | 2.8 | ‰ | 0.8× | |
| ε_c2 Strain at peak, parabola–rectangle | 2 | 2.5 | ‰ | 1.25× | |
| ε_cu2 Ultimate strain, parabola–rectangle | 3.5 | 2.6 | ‰ | 0.743× | |
| n Exponent, parabola–rectangle | 2 | 1.4 | – | 0.7× | |
| ε_c3 Strain at peak, bilinear | 1.75 | 2.2 | ‰ | 1.26× | |
| ε_cu3 Ultimate strain, bilinear | 3.5 | 2.6 | ‰ | 0.743× | |
| E/ρ Specific stiffness E/ρ · derived | 14.71 | 17.16 | MJ/kg | 1.17× | |
| c₀ Bar wave speed √(E/ρ) · derived | 3835 | 4143 | m/s | 1.08× | |
| f/ρ Specific strength f/ρ · derived | 18.39 | 32.69 | kJ/kg | 1.78× |