C20/25 vs C70/85
C70/85 is 1.4 times as stiff as C20/25. Their densities are about the same. Per unit mass C70/85 is 1.4 times as stiff. Strength: f_ck = 20 MPa for C20/25, f_ck = 70 MPa for C70/85.
Side by side
ratio = C70/85 / C20/25 · log scale| Property | C20/25 | C70/85 | Unit | Ratio | ¼×1×4× |
|---|---|---|---|---|---|
| E Young's modulus | 30 | 41 | GPa | 1.37× | |
| G Shear modulus | 12.5 | 17.08 | GPa | 1.37× | |
| ν Poisson's ratio | 0.2 | 0.2 | – | 1× | |
| ρ Density | 2447 | 2447 | kg/m³ | 1× | |
| γ Weight density | 24 | 24 | kN/m³ | 1× | |
| α Coefficient of thermal expansion | 10 | 10 | 10⁻⁶/K | 1× | |
| f_ck Characteristic cylinder strength | 20 | 70 | MPa | 3.5× | |
| f_ck,cube Characteristic cube strength | 25 | 85 | MPa | 3.4× | |
| f_cm Mean cylinder strength | 28 | 78 | MPa | 2.79× | |
| f_ctm Mean tensile strength | 2.2 | 4.6 | MPa | 2.09× | |
| f_ctk,0.05 Tensile strength, 5 % fractile | 1.5 | 3.2 | MPa | 2.13× | |
| f_ctk,0.95 Tensile strength, 95 % fractile | 2.9 | 6 | MPa | 2.07× | |
| ε_c1 Strain at peak stress | 2 | 2.7 | ‰ | 1.35× | |
| ε_cu1 Ultimate strain | 3.5 | 2.8 | ‰ | 0.8× | |
| ε_c2 Strain at peak, parabola–rectangle | 2 | 2.4 | ‰ | 1.2× | |
| ε_cu2 Ultimate strain, parabola–rectangle | 3.5 | 2.7 | ‰ | 0.771× | |
| n Exponent, parabola–rectangle | 2 | 1.45 | – | 0.725× | |
| ε_c3 Strain at peak, bilinear | 1.75 | 2 | ‰ | 1.14× | |
| ε_cu3 Ultimate strain, bilinear | 3.5 | 2.7 | ‰ | 0.771× | |
| E/ρ Specific stiffness E/ρ · derived | 12.26 | 16.75 | MJ/kg | 1.37× | |
| c₀ Bar wave speed √(E/ρ) · derived | 3501 | 4093 | m/s | 1.17× | |
| f/ρ Specific strength f/ρ · derived | 8.172 | 28.6 | kJ/kg | 3.5× |
Values at the first thickness band or product form of each material (EN 1992-1-1; EN 1992-1-1). A minimum and a characteristic value are not the same kind of number — read the ratio as a guide. Each material's page lists every band and every source.