EN AW-6106 T6 and EN AW-6082 T6 are about equally stiff. Their densities are about the same. Per unit mass they are about equally stiff (25.93 and 25.93 MJ/kg). Strength: f_o = 250 MPa for EN AW-6082 T6, f_o = 200 MPa for EN AW-6106 T6.
f_o,haz 0.2 % proof strength in the heat-affected zone
125
95
MPa
0.76×
f_u,haz Tensile strength in the heat-affected zone
185
160
MPa
0.865×
E/ρ Specific stiffness E/ρ · derived
25.93
25.93
MJ/kg
1×
c₀ Bar wave speed √(E/ρ) · derived
5092
5092
m/s
1×
f/ρ Specific strength f/ρ · derived
92.59
74.07
kJ/kg
0.8×
Values at the first thickness band or product form of each material (EN 1999-1-1 · t ≤ 5 mm · EP/O, EP/H, ET; EN 1999-1-1 · t ≤ 10 mm · EP). A minimum and a characteristic value are not the same kind of number — read the ratio as a guide. Each material's page lists every band and every source.
COOKIES
We use a few cookies to see which pages engineers actually read and where they get stuck, and to tell whether our Google Search ads led to a sign-up or a purchase. No retargeting, nothing that follows you to other sites. They only start if you accept; reject and they stay off, and the site works exactly the same.