EN AW-6060 T5 vs EN AW-6060 T6
EN AW-6060 T6 and EN AW-6060 T5 are about equally stiff. Their densities are about the same. Per unit mass they are about equally stiff (25.93 and 25.93 MJ/kg). Strength: f_o = 120 MPa for EN AW-6060 T5, f_o = 140 MPa for EN AW-6060 T6.
Side by side
ratio = EN AW-6060 T6 / EN AW-6060 T5 · log scale| Property | EN AW-6060 T5 | EN AW-6060 T6 | Unit | Ratio | ¼×1×4× |
|---|---|---|---|---|---|
| E Young's modulus | 70 | 70 | GPa | 1× | |
| G Shear modulus | 27 | 27 | GPa | 1× | |
| ν Poisson's ratio | 0.3 | 0.3 | – | 1× | |
| ρ Density | 2700 | 2700 | kg/m³ | 1× | |
| α Coefficient of thermal expansion | 23 | 23 | 10⁻⁶/K | 1× | |
| f_u Tensile strength (R_m) | 160 | 170 | MPa | 1.06× | |
| f_o 0.2 % proof strength | 120 | 140 | MPa | 1.17× | |
| f_o,haz 0.2 % proof strength in the heat-affected zone | 50 | 60 | MPa | 1.2× | |
| f_u,haz Tensile strength in the heat-affected zone | 80 | 100 | MPa | 1.25× | |
| E/ρ Specific stiffness E/ρ · derived | 25.93 | 25.93 | MJ/kg | 1× | |
| c₀ Bar wave speed √(E/ρ) · derived | 5092 | 5092 | m/s | 1× | |
| f/ρ Specific strength f/ρ · derived | 44.44 | 51.85 | kJ/kg | 1.17× |
Values at the first thickness band or product form of each material (EN 1999-1-1 · t ≤ 5 mm · EP, ET, ER/B; EN 1999-1-1 · t ≤ 15 mm · EP, ET, ER/B). A minimum and a characteristic value are not the same kind of number — read the ratio as a guide. Each material's page lists every band and every source.