Material library

A sourced material library for structural analysis: strength by thickness and product form, elastic constants — orthotropic where the material is — density, thermal and electrical properties. Every value names its source and says what kind of value it is; the whole library downloads as JSON.

FREE · NO SIGN-UP v2.0.0 · verified against 14 reference cases
LIBRARY99 materials
1 · Find a material
2 · Thickness and product form for values that depend on them
Download the whole library · JSON

The JSON is the library's exchange format: SI units, the basis and source of every value. Tessera imports the same file.

Structural steel · EN 10025-2

S355

isotropic · hot rolled, non-alloy
  • EN 1993-1-1 3.2.1 lets the design take f_y = R_eH and f_u = R_m,min from EN 10025-2, or the simplified values of its Table 3.1; the National Annex may choose.
Free with an account · Sign in

HOW IT'S CALCULATED · WITH YOUR NUMBERS

Step by step, with your numbers

EN 10025-2, EN 1993-1-1/-1-2/-1-4, EN 10088-1, EN 1999-1-1, EN 1992-1-1, EN 1991-1-1, EN 338, EN 14080; producer datasheets and composite textbooks for typical values.

BEYOND THE MINIMUM VALUES

Material testing data, temperature-dependent and non-linear material models — we build them into the analysis.

Submit a Problem →

More calculators